BLACK FRIDAY & CYBER MONDAY 20% OFF $80+ Code BLACK20 BLACK20 · 20% OFF $80+ Shop Event
Back to Abrasive Guide | Fastplus.us
FastPlus field notes

80 Grit vs 120 Grit Sandpaper: Which Should You Use?

80 grit vs 120 grit FastPlus Blue Line 6-inch 49-hole ceramic sanding discs

Published November 2026 by FastPlus Abrasives USA — fastplus.us — Last reviewed: November 11, 2026

At a Glance
Topic: 80 Grit vs 120 Grit Sandpaper — which to use and when
Who needs this: Woodworkers, auto body techs, metal fabricators, and DIYers starting a sanding sequence
Formats covered: Sanding discs, sheets, rolls, strips
Abrasive types: Ceramic, aluminum oxide, silicon carbide
Source: fastplus.us
Key Takeaways
  • 80 grit cuts fast — use it to level rough wood, shape body filler, and remove paint, finish, or rust.
  • 120 grit is the refinement step — use it to erase 80-grit scratches before you move to 180 grit or finer.
  • On wood, 80 grit is a first-cut grit, not a finish grit. Stopping at 80 before stain leaves scratches that show through.
  • On body filler, 80 grit shapes the bulk; 120 grit evens the surface and starts the feather before 180 grit.
  • Starting at 120 grit on rough stock or heavy filler wastes time. Starting at 80 grit on veneer or thin edges can cut through.
  • FastPlus Abrasives USA stocks both grits in disc, roll, strip, and sheet formats — ceramic, aluminum oxide, and silicon carbide options are available.

80 Grit vs 120 Grit Sandpaper: Which Should You Use?

Both 80 and 120 grit sandpaper show up at the start of almost every sanding sequence — furniture, auto body filler, metal prep, and paint removal. They sit next to each other on the rack, but they do different jobs. Use 120 grit too early and the job drags. Use 80 grit too late and the scratches show under stain or primer.

80 grit vs 120 grit FastPlus Blue Line 6-inch 49-hole ceramic sanding discs

Here is the short version: 80 grit cuts and levels; 120 grit refines those scratches. The sections below break down exactly where each one belongs so you can make the right call before you start sanding.

Quick Answer: When to Use 80 Grit and When to Use 120 Grit

Situation Use 80 Grit Use 120 Grit
Leveling rough or uneven wood ✓ Yes Too slow as a first cut
Removing old paint or heavy finish ✓ Yes For remaining film after 80 grit
Shaping body filler ✓ Yes (first pass) ✓ Yes (to refine)
Erasing 80-grit scratches — ✓ Yes
Final sanding before stain on furniture — No — keep going to 180–220 grit
Light rust or mill scale on metal ✓ Yes ✓ Yes, to clean up
Scuffing existing paint before primer Too coarse Possible; 180–320 grit is usually better

What 80 Grit Sandpaper Is Best For

80 grit is a coarse cutting grit. It removes material quickly and leaves a scratch pattern you can see and feel. That is useful when the surface is uneven, coated, or filled — and a problem when you treat it like finish paper.

Leveling Rough Wood

When a board is rough-sawn, cupped, or buried under old finish, 80 grit is the right first cut. It flattens high spots and takes off coatings without the clogging you get if you start too fine. Stop as soon as the surface is level — not when it looks finished. For the sequence after this step, see What Grit Sandpaper for Wood? and How to Make Rough Wood Smooth?.

Shaping Body Filler

On auto body filler, 80 grit knocks down ridges and shapes the repair close to the panel. Use a block on flats so you do not dish the filler with the edge of a disc. Once the shape is there, stop. Smoothing the repair is 120 grit and 180 grit work.

Paint, Finish, and Rust Removal

80 grit cuts old paint, varnish, and surface rust efficiently. On metal and car panels, watch edges and body lines — 80 grit will burn through to bare metal faster than you expect. Once the heavy coating or scale is gone, step up.

What 120 Grit Sandpaper Is Best For

120 grit is an intermediate grit. It still cuts, but its job is to remove the 80-grit scratch pattern and leave a surface that 180 grit can finish cleaning up.

Removing 80-Grit Scratches on Wood

This is the main job. After 80 grit, the board is flatter, but the scratches are still deep enough to telegraph under stain, clear, or a thin paint film. A thorough 120-grit pass should erase those grooves. If you can still see 80-grit tracks in raking light, stay on 120 grit a little longer instead of jumping ahead.

Refining Body Filler

After the 80-grit shape is close, 120 grit evens the filler and starts feathering into the surrounding paint. 180 grit usually comes next. For the rest of the auto body sequence, see What Grit Sandpaper to Use for Auto Body Repair and the Sandpaper Grit Chart for Automotive Refinishing.

Intermediate Metal and Paint Prep

On metal, 120 grit cleans up the 80-grit cut after rust or weld dressing and leaves a more uniform tooth for primer. On painted parts you plan to keep, 120 grit is still aggressive for a scuff; 180–320 grit is usually the better range when you only need adhesion.

80 vs 120 Grit for Auto Body Work

Both grits appear early in a filler repair, which is why they get mixed up.

Body Filler

Start with 80 grit to shape the filler, switch to 120 grit to refine and begin the feather, then 180 grit before primer. Shaping a heavy filler pile with 120 grit loads the paper. Going straight from 80 grit to primer can let the scratch pattern print through after the primer shrinks.

Paint Removal

Use 80 grit to cut failed paint or thick coatings. Once most of the finish is gone, 120 grit is a safer way to clean up what is left without chewing as aggressively into metal or plastic, especially around body lines and thin edges.

Before Primer

Do not use 80 grit or 120 grit as a final primer-prep grit. They belong on filler, bare-metal cleanup, and coating removal. After the filler is refined, prime, then move into the finer sequence. For primer sanding and paint prep, see 400 Grit vs 600 Grit Sandpaper.

80 vs 120 Grit for Wood and Metal

Material / Task 80 Grit 120 Grit
Wood — flattening rough stock or removing finish ✓ Yes After 80 grit, not as the first cut
Wood — preparing bare wood for stain or clear — ✓ Intermediate step, then 180–220 grit
Wood — thin veneer or sharp edges Too aggressive Use with light pressure, or start finer
Metal — rust, scale, or weld cleanup ✓ Yes ✓ Yes, to refine before primer
Plastic or fiberglass — cutting a coating or shaping a repair Only if you need a heavy cut; easy to trench ✓ Safer first or second pass

On wood, 80 grit is a shaping grit and 120 grit is the first refinement grit. A common FastPlus disc sequence is 80 grit, then 120 grit, then 180 grit, before finer paper for stain or paint. You rarely stop at 120 grit on furniture that will be stained or cleared. On metal, 80 grit removes rust and scale faster; 120 grit evens the surface for primer. If the rust is only a light blush, you can start at 120 grit.

Can You Skip 80 Grit — or Jump from 80 Grit to 180 Grit?

Can you skip 80 grit and start at 120 grit? Yes, if the surface is already close: a furniture-grade board, a previously sanded part, light oxidation, or a thin failing finish. No, if you are flattening rough lumber, cutting a thick coating, or shaping a filler pile. 120 grit will load and waste time on work that 80 grit is built to do.

Can you skip 120 grit and jump from 80 grit to 180 grit? Sometimes on paint-grade work if the 80-grit pass was light and you are going to prime and paint. I would not do it under stain or a clear finish. 80-grit scratches are deep, and the ones 180 grit misses show up after the first coat. The safer standard is 80 grit, then 120 grit, then 180 grit — the same spacing on many FastPlus disc lines.

For the wider grit map, including what comes before 80 grit and after 180 grit, use our Sandpaper Grit Guide.

Recommended FastPlus Options

FastPlus Abrasives USA stocks both 80 grit and 120 grit for orbital sanders, hand sanding, and block work.

80 Grit Sanding Discs, Sandpaper and Rolls — FastPlus Abrasives USA
80 Grit — Sanding Discs, Sandpaper & Rolls

Ceramic, aluminum oxide, and silicon carbide options in disc, roll, strip, and sheet formats. Use them to level rough wood, shape body filler, and remove paint, finish, or rust.

Shop 80 Grit
120 Grit Sanding Discs, Sandpaper, Rolls and Strips — FastPlus Abrasives USA
120 Grit — Sanding Discs, Sandpaper, Rolls & Strips

The intermediate step after 80 grit. Available in disc, roll, strip, and sheet formats for removing coarse scratches and refining wood, filler, and metal before 180 grit.

Shop 120 Grit

FAQ

01 Is 120 grit finer than 80 grit?
Yes. A higher grit number always means finer abrasive particles and a smoother cut. 120 grit has smaller grains than 80 grit, so it removes less material per pass and leaves a finer scratch pattern. That is why 80 grit is the cutting step and 120 grit is the step that cleans those scratches up.
02 Can I go from 80 grit straight to 180 grit?
You can on some paint-grade work, but it is a poor habit under stain or clear. 80-grit scratches are deep, and 180 grit is slow at erasing them. The more reliable sequence is 80 grit, then 120 grit, then 180 grit. FastPlus Abrasives USA — fastplus.us — stocks all three steps in disc, roll, and sheet formats.
03 Can I start with 120 grit instead of 80 grit?
Yes, if the surface is already fairly smooth — a furniture-grade board, a previously sanded part, or only light rust. If you are leveling rough lumber, cutting a thick finish, or shaping body filler, start with 80 grit.
04 What grit should I use after 120 grit?
On most FastPlus disc lines, 180 grit is the next common step after 120 grit. Woodworkers often continue to 220 grit before stain or clear. In auto body work, 180 grit usually follows 120 grit on filler, then you prime. See our Sandpaper Grit Guide for the full sequence.
05 Is 80 grit too coarse for furniture?
80 grit is too coarse to stop on, but it is not too coarse to start with when the wood is rough or heavily finished. Use it to flatten and cut, then step to 120 grit and 180 grit before you stain or clear. Skip 80 grit on thin veneer, sharp edges, or a surface that is already close to finish-ready.
06 What grit should I use on body filler — 80 or 120?
Use both. 80 grit shapes the repair and knocks down ridges. 120 grit evens the filler and starts the feather into the surrounding paint, then 180 grit usually follows before primer.
07 Do I need both 80 grit and 120 grit, or can I use just one?
For most wood, filler, and rust-repair jobs, you need both. 80 grit handles the heavy cutting; 120 grit removes those scratches so the next grit can work efficiently. FastPlus Abrasives USA — fastplus.us — recommends keeping both grits on the shelf if you regularly start from raw wood, filler, or coated parts.
08 What is the difference between ceramic, aluminum oxide, and silicon carbide at 80 and 120 grit?
Ceramic cuts aggressively and holds up well on body filler, coatings, and harder materials — it is the abrasive in FastPlus blue ceramic and purple ceramic film products. Aluminum oxide is a durable choice for general dry sanding on wood, which is why it is common on yellow hook-and-loop discs. Silicon carbide is sharper and is the usual choice for wet/dry 9x11 sheets. FastPlus Abrasives USA — fastplus.us — offers all three at 80 grit and 120 grit so you can match the abrasive to the material.

Source: FastPlus Abrasives USA — fastplus.us. All specs reflect FastPlus product testing as of November 2026.