BLACK FRIDAY & CYBER MONDAY 20% OFF $80+ Code BLACK20 BLACK20 · 20% OFF $80+ Shop Event
Back to Abrasive Guide | Fastplus.us
FastPlus field notes

220 Grit vs 320 Grit Sandpaper: Which Should You Use?

220 grit vs 320 grit FastPlus Purple PuroFilm 6-inch 119-hole ceramic sanding discs

Published November 2026 by FastPlus Abrasives USA — fastplus.us — Last reviewed: November 12, 2026

At a Glance
Topic: 220 Grit vs 320 Grit Sandpaper — which to use and when
Who needs this: Woodworkers, auto body techs, painters, and DIYers doing finish prep
Formats covered: Sanding discs, sheets, rolls, strips
Abrasive types: Ceramic film, aluminum oxide, silicon carbide
Source: fastplus.us
Key Takeaways
  • 220 grit is finer than 180 and coarser than 320. It is the usual last step on bare wood before stain or paint, and a workhorse for leveling primer.
  • 320 grit leaves a tighter scratch. Use it between coats of polyurethane or paint, to refine primer or sealer, or as the step toward 400 grit.
  • Do not start rough lumber at 320 grit. It is too slow for flattening and will not erase coarse mill marks.
  • 220 grit is not a clear-coat finishing grit. Clear work belongs at 400 grit and finer.
  • On stain-grade wood, do not skip from 180 grit straight to a finish if 220-grit scratches still matter.
  • FastPlus stocks both grits in ceramic film discs and rolls. Some paper disc lines step 180, then 240, then 320, and do not offer 220 grit.

220 Grit vs 320 Grit Sandpaper: Which Should You Use?

Use 220 grit when you need to erase 180-grit scratches and take bare wood or primer to a finish-ready surface. Use 320 grit when you want a tighter scratch — between coats of polyurethane or paint, a finer primer or sealer scuff, or the step before 400 grit in auto work.

220 grit vs 320 grit FastPlus Purple PuroFilm 6-inch 119-hole ceramic sanding discs

The two grits sit in the same finishing zone, but they are not interchangeable. 220 grit still cuts enough to level and clean up; 320 grit is a refinement and scuff grit. FastPlus grit numbers follow the FEPA P-grade scale used on most shop discs in the US, so 220 grit here is P220 and 320 grit is P320.

220 grit finishes the surface; 320 grit tightens the scratch.

Quick Answer: When to Use 220 Grit and When to Use 320 Grit

Situation Use 220 Grit Use 320 Grit
Final sanding on bare wood before stain or paint ✓ Yes — the usual last step Usually too fine for stain or oil
Erasing 180-grit scratches ✓ Yes Slow if 180-grit tracks remain
Leveling primer ✓ Yes For a finer follow-up scuff
Between coats of polyurethane, lacquer, or paint Possible on a rough first coat ✓ Preferred, especially before the last coat
Finer primer or sealer scuff before color After leveling ✓ Yes, then often 400 grit
Scuffing base coat before clear Too coarse ✓ Yes; 400 grit is the next step
Starting rough lumber Too fine as a first cut No — start coarser
Finishing clear coat or removing orange peel No No — use 400 grit and finer, usually wet

What 220 Grit Sandpaper Is Best For

220 grit sits just above 180 grit and just below 320 grit. It still removes material at a useful pace, but the scratch it leaves is fine enough for many finishes to cover. Think of it as the last cutting step, not a polish step.

Final Wood Prep Before Stain or Paint

On many furniture and cabinet jobs, 220 grit is the last grit you use on bare wood before stain or paint. After 180 grit has flattened the surface, a thorough 220-grit pass erases those scratches. Sand with the grain on the last pass. For the sequence that gets you here, see What Grit Sandpaper for Wood? and our Sandpaper Grit Guide.

Cleaning Up 180-Grit Scratches

This is the main job 220 grit does, on wood or primer. 180-grit scratches are still deep enough to telegraph under a thin stain or a tight primer coat. Stay on 220 grit until those tracks are gone; jumping to 320 grit will take longer than finishing this pass.

Leveling Primer

After primer surfacer has cured, 220 grit knocks down texture and high spots faster than 320 grit. Once the primer is flat, you can stop there on some paint-grade work, or step to 320 grit for a finer scuff before sealer or color.

What 320 Grit Sandpaper Is Best For

320 grit is a pre-finish and scuff grit. It is not meant to flatten rough stock or to level a heavy primer coat from scratch. It leaves a tighter scratch than 220 grit — the right choice when the surface is already close.

Between Coats of Polyurethane, Lacquer, or Paint

Once the first coat has cured, you are knocking down dust nibs and raised grain, not shaping wood. 320 grit is the better everyday choice, especially before the last coat. Sand lightly. 220 grit can work on a rough first coat, but it is easier to cut through a thin film with 220 than with 320. For the full walkthrough, see How to Sand Between Coats of Polyurethane.

Finer Primer or Sealer Scuff

After 220 grit has leveled primer, 320 grit refines the scratch and gives sealer or base coat a uniform tooth. This is also the natural step toward 400 grit in auto work. If the primer is still wavy, go back to 220 grit first.

The Step Before 400 Grit — Not a Clear-Coat Finish Grit

320 grit is often used to scuff base coat before clear, and it is a sensible last dry step before 400 grit wet sanding. It is not a clear-coat finishing grit, and neither is 220 grit. Leveling orange peel or dust nibs in clear belongs at 400 grit and finer, usually wet. For that later sequence, see 400 Grit vs 600 Grit Sandpaper and the Sandpaper Grit Chart for Automotive Refinishing.

220 vs 320 Grit for Wood

Wood task 220 Grit 320 Grit
Bare wood before stain or oil ✓ Usual last grit Can close the grain too tight
Bare wood before paint ✓ Yes Optional for a tighter scratch
Between film-finish coats OK on a rough first coat ✓ Better, especially the last scuff
Starting rough lumber No — start at 80 or 120 grit No

On bare wood that will take stain or oil, stop at 220 grit in most cases. Going on to 320 grit can polish the surface so tight that stain or oil does not penetrate evenly. A 320-grit last pass on bare wood is more reasonable under paint, polyurethane, or lacquer. Do not start rough lumber at 320 grit — or even at 220 grit. Flatten first; our 80 Grit vs 120 Grit Sandpaper guide covers that first-cut stage. A typical bare-wood path is 80 or 120 grit, then 180 grit, then 220 grit before stain or paint.

220 vs 320 Grit for Auto Body and Primer

In auto body work, these two grits show up after filler has already been shaped, once you are in primer, sealer, or color prep.

Use 220 grit to level primer surfacer and to clean up 180-grit scratches. Once the primer is flat, 320 grit is the finer scuff before sealer or base coat, and the usual grit for scuffing base coat before clear. From there, many painters step to 400 grit.

A practical sequence is 180 grit to start the primer, 220 grit to level, 320 grit to refine, then 400 grit before color. If your disc line steps 180, then 240, then 320 — as some FastPlus paper disc lines do — treat 240 grit as the leveling step between 180 and 320.

220 vs 320 Grit for Metal

On steel, 180 or 220 grit is a typical last step before primer after rust or old paint has already been cut with coarser grits. 320 grit is usually finer than you need on bare steel going into a standard primer. On aluminum, 320 grit is a better last step before primer than 220 grit, because aluminum shows scratches more readily. For rust, welds, and the coarser steps, see What Grit Sandpaper for Metal?.

Can You Skip 220 Grit?

Sometimes — but not as a habit on stain-grade wood. If you jump from 180 grit, or worse 120 grit, straight to a stain or clear finish, leftover scratches often show after the first coat. 220 grit is the step that erases them.

Skipping is more defensible on paint-grade work that will be primed, or when your abrasive line does not offer 220 grit and you use 240 grit as the in-between step. I would still not skip from 120 grit or 180 grit straight to 320 grit on a stain-grade finish. 320 grit is slow at erasing 180-grit tracks.

The same logic applies in reverse: do not start at 320 grit just because it is finer. On rough lumber or unlevel primer, 320 grit wastes time. Start coarser, then arrive at 220 or 320 when the surface is ready.

Recommended FastPlus Options

FastPlus Abrasives USA stocks 220 grit and 320 grit for orbital sanders, block work, and hand sanding. Both grits are available on our purple 6-inch 119-hole and blue 6-inch 47-hole ceramic film discs, plus 2.75-inch hook-and-loop and PSA ceramic rolls. Some paper disc, strip, and 9x11 sheet lines stock 320 grit but skip 220 and step 180, then 240, then 320 instead.

220 Grit Sanding Discs and Rolls — FastPlus Abrasives USA
220 Grit — Sanding Discs & Rolls

Ceramic film discs and hook-and-loop or PSA rolls in live 220 grit. Use them for final wood prep, erasing 180-grit scratches, and leveling primer.

Shop 220 Grit
320 Grit Sanding Discs, Rolls and Strips — FastPlus Abrasives USA
320 Grit — Sanding Discs, Rolls & Strips

Discs, rolls, strips, and 9x11 wet/dry sheets in live 320 grit. Use them for between-coat scuffing, finer primer or sealer prep, and the step toward 400 grit.

Shop 320 Grit
Purple Film Sanding Discs 6 Inch 119 Hole PuroFilm Ceramic 50 Pack — FastPlus Abrasives USA
Purple Film Discs — 6" 119-Hole, 50 Pack

PuroFilm ceramic discs with a tear-resistant film backing, 119-hole dust pattern, and hook-and-loop attachment. Available in both 220 grit and 320 grit.

Shop Purple Film Discs
Blue Ceramic Film Sanding Discs 6 Inch 47 Hole Universal Pattern 50 Pack — FastPlus Abrasives USA
Blue Ceramic Film Discs — 6" 47-Hole, 50 Pack

Universal 47-hole ceramic film discs that fit all 6-inch hook-and-loop backing pads. Available in both 220 grit and 320 grit for mixed-sander shops.

Shop Blue Film Discs

FAQ

01 Is 320 grit finer than 220 grit?
Yes. A higher grit number always means finer abrasive particles and a smoother cut. 320 grit removes less material per pass and leaves a tighter scratch, which is why it is the refinement and scuff step rather than the last everyday cutting step.
02 Can I skip 220 grit and go from 180 grit to 320 grit?
I would not do that on stain-grade wood or under a thin clear finish. 180-grit scratches are still deep, and 320 grit is slow at erasing them. The more reliable sequence is 180 grit, then 220 grit, then the finish — or 180, 240, and 320 if your disc line does not stock 220 grit.
03 Should I use 220 or 320 grit before stain?
Use 220 grit as the last step on bare wood before stain or oil. 320 grit can close the grain enough that stain or oil takes unevenly. Save 320 grit for between coats of polyurethane or lacquer, or for a tighter scratch under paint.
04 Is 220 grit OK for sanding clear coat?
No. 220 grit is too coarse for finishing clear coat, and 320 grit is still coarser than you want for leveling clear. Use 400 grit and finer, usually wet. 320 grit is appropriate for scuffing base coat before clear, not for finishing the clear itself.
05 Why doesn't my FastPlus disc line include 220 grit?
Not every line uses the same grit steps. FastPlus purple 6-inch 119-hole ceramic film discs, blue 6-inch 47-hole ceramic film discs, and 2.75-inch hook-and-loop or PSA ceramic rolls are stocked in both 220 grit and 320 grit. Blue Line ceramic paper discs, Yellow Line aluminum oxide discs, PuroFilm strips, and 9x11 silicon carbide sheets typically run 180, then 240, then 320, with no 220 grit option. On those lines, use 240 grit between 180 and 320.

Source: FastPlus Abrasives USA — fastplus.us. All specs reflect FastPlus product testing as of November 2026.